钢丝绳输送带的检测方式有哪些?

来源:http://www.huafengxiangsu.com 时间:2019-07-17 10:31:12 浏览次数:0
  钢丝绳保送带探伤的检测办法有哪些呢?下面就有大倾角输送带厂家给大家引见一下,希望我们的引见能够更好的帮到你们。
  What are the detection methods of wire rope belts? Below there are the manufacturers of the belts to introduce to you, I hope our introduction can better help you.
  1、简易接头变形检测法:简易接头变形检测法即传统的人工检查办法,就是现场维修人员用眼睛直接察看皮带外形,判别皮带接头能否伸长,再辅助运用便携式x光照相的办法,对皮带的坏损停止检测,主要有以下3种办法。
  1. Simple Joint Deformation Detection Method: Simple Joint Deformation Detection Method is the traditional manual inspection method, that is, on-site maintenance personnel use their eyes to directly inspect the shape of the belt, to determine whether the belt joint can be elongated, and then assist the use of portable X-ray photography method to stop the detection of belt damage, there are three main methods.
  2、“起泡”现象观测法L4J。“起泡”现象是接头损伤常见的一种毛病特征,其缘由是起泡部位的钢绳芯抽动所致。这是一种常被我国煤矿现场运用的简易检测法,即在停机后肃清接头区的胶带外表,查看有无“起泡”现象发作,一旦发现有起泡现象,便予以留意,当起泡区域开展到全带宽的l/3时,则立即予以更新处置。
  2. Blistering phenomenon observation method L4J. Bubble phenomenon is a common defect characteristic of joint damage, which is caused by the pulling of steel rope core at the bubbling part. This is a simple detection method which is often used in coal mines in our country. It is to clean the surface of the tape in the joint area after shutdown to check whether there is a "blistering" phenomenon. Once a blistering phenomenon is found, it will be noticed. When the blistering area reaches 1/3 of the full bandwidth, it will be updated and disposed of immediately.
钢丝绳输送带的检测方式有哪些
  3、接头长度丈量法。在刚做好的硫化接头两边境恰当位置,等间隔地刻划3组标志线,并量取每组标志线的长度。胶带投入运用后,定期地丈量每条标志线的长度,当发现三者中恣意一个的伸长量超越某一阈值时,就用X射线探测仪对该硫化接头停止拍片剖析,以肯定该接头的损坏水平以及能否继续运用。
  3. Joint length measurement method. Three groups of marking lines are carved at equal intervals in the proper position of the two borders of the newly made vulcanized joints, and the length of each group of marking lines is measured. After the tape is put into use, the length of each marking line is measured regularly. When it is found that the elongation of one of the three marking lines exceeds a certain threshold, X-ray detector is used to stop the film analysis of the vulcanized joint in order to confirm the damage level of the joint and whether it can continue to be used.
  经过保送带厂家给大家引见钢丝绳保送带探伤的检测办法你理解了吗?想学习更多保送带的学问请继续关注我们:https://www.huafengxiangsu.com
  After the belt manufacturers to introduce to you the wire rope belt flaw detection method, do you understand? If you want to learn more about the delivery belt, please continue to pay attention to us: https://www.huafengxiangsu.com